Forging A Polled Tomahawk By Butch Sheely Article from "American Bladesmith" Spring 2010

#1 User is online   ABS Webmaster 

  • Administrator
  • Icon
  • View gallery
  • Group: Administrators
  • Posts: 908
  • Joined: 21-December 09
  • LocationSalida, Colorado
  • ABS Rating:Journeyman Smith

Posted 30 June 2010 - 02:54 PM

Forging a Polled Tomahawk


Butch Sheely, Journeyman Smith, wrote an excellent article entitled "Forging a Polled Tomahawk" that appeared in the "American Bladesmith" which is the Journal of the American Bladesmith Society and was published in the Spring 2010 issue. The article describes the materials needed and step by step instructions that include diagrams.

Attached Image


A PDF copy of the article can be dowloaded by clicking: "Forging a Polled Tomahawk by Butch Sheely".

Dan Cassidy
ABS Webmaster and Forum Administrator

Send an email to Dan

Posted Image


0

#2 User is offline   Rick Baum 

  • Advanced Forum Member
  • PipPipPipPip
  • Group: Members
  • Posts: 168
  • Joined: 11-March 10
  • LocationIdaho (Boise)
  • ABS Rating:Apprentice Smith

Posted 01 July 2010 - 07:17 PM

Thanks for posting this Dan! I haven't made a tomahawk yet. I can't wait to try it out.

Make sure that Butch knows his contribution is appreciated if he's not on the forum very often.

Rick
0

#3 User is offline   Neels_VanDenBerg 

  • New Forum Member
  • Pip
  • Group: Members
  • Posts: 1
  • Joined: 18-October 12
  • LocationPretoria, South Africa
  • ABS Rating:Apprentice Smith

Posted 21 November 2012 - 07:45 AM

This is brilliant! Thank you all for sharing ... ;)
0

#4 User is offline   Brian Thie 

  • Advanced Forum Member
  • PipPipPipPip
  • View gallery
  • Group: Members
  • Posts: 163
  • Joined: 10-March 10
  • LocationBurlington, Iowa
  • ABS Rating:Journeyman Smith

Posted 21 November 2012 - 10:53 AM

Butch is an excellent hawk maker and this is a great article.

I highly suggest going to the Mid-America Bladesmithing Symposium held in Troy Ohio usually at the end of August. Butch often demonstrates his hawk making skills there. Butch makes many styles of hawks and watching him make a hawk from a strap of steel, wrapping it around a drift, welding together and welding in a bit is just shy of magical. I have learned a lot by just watching Butch's techniques when doing demos like this.

Brian
Brian Thie
Journeyman Smith
www.mepotelco.net/web/tknives