American Bladesmith Society Forum: Anvils? - American Bladesmith Society Forum

Jump to content

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

Anvils?

#1 User is offline   jared_foster 

  • Advanced Forum Member
  • PipPipPipPip
  • Group: Members
  • Posts: 84
  • Joined: 20-December 11
  • LocationColorado City, TX
  • ABS Rating:Apprentice Smith

Posted 30 July 2012 - 02:26 PM

Does anyone use a post type anvil? I am currently making one out of the bottom of a railroad rail and some 4" square tubing. Any ideas for tooling etc. I started making it because neither of my current two anvils has square corners for creating the pinch at the recasso. Also any pointers for making it last?
0

#2 User is offline   justin carnecchia 

  • Advanced Forum Member
  • PipPipPipPip
  • Group: Members
  • Posts: 76
  • Joined: 06-April 11
  • LocationSandpoint ID
  • ABS Rating:Apprentice Smith

Posted 02 August 2012 - 07:37 AM

For a long time I used a 3ft piece of track stood on end. The good part was that it put a lot of mass directly under the work piece, on the down side it only offered a few inches of flat surface (for most things it was plenty but it is nice to have a bigger surface for straightening), and it isn't hardened. I know you can harden it but that was a bigger job than I wanted to mess with. I'm having a hard time envisioning what you are thinking but the biggest problem I would see with using the bottom of the rail is having enough mass under your work. If you already have two anvils and are just looking for a sharp edge you might want to consider just using the end, to keep it stable I put it in a bucket filled with sand.

The "Anvilfire" web site has a page on railroad track anvils you might want to look at, as I recall they were all based on standing the track on end.
justin carnecchia
Apprentice Smith
0

#3 User is offline   Steve Seib 

  • Forum Member
  • PipPip
  • Group: Members
  • Posts: 7
  • Joined: 17-June 10
  • LocationEvansville, IN
  • ABS Rating:Apprentice Smith

Posted 02 August 2012 - 09:47 AM

Jared,

If your anvil has a hardie hole and just doesn't have good corners for pinching out the cutting edge, check this bottom set out at Blacksmith's Depot.

https://www.blacksmi...nvil_Block.xml/

I do some demo's at the local antique club show and the county fair, our anvils are sway-backed and edges rounded or broken-out so I made one similar to the one at the link for when I demo knives at the shows. You could also go with a guillotine type tool or a spring fuller type tool to accomplish creating the initial pinch.

https://www.blacksmi...Fuller_Kit.xml/

Hope that helps.

Steve Seib
0

#4 User is offline   jared_foster 

  • Advanced Forum Member
  • PipPipPipPip
  • Group: Members
  • Posts: 84
  • Joined: 20-December 11
  • LocationColorado City, TX
  • ABS Rating:Apprentice Smith

Posted 03 August 2012 - 02:58 PM

Thanks guys. What I ended up doing was taking some 1/4" thick X4" square tubing that is three foot long and stood it on end. Then I cut off the bottom of a railroad rail and welded it on the top end. Then I cemented the tubing into a 30 gallon drum with reinforced concrete to get the weight up. I don't know how or where Don Fogg got or made his post anvil but that is kind of what I am trying to reproduce. You can see his in some of the pictures on his website.