Posted 03 June 2012 - 08:32 AM

Thought I might toss in a hot-bluing video.
I started bluing my Damascus and steel fittings more than a decade ago and have never turned back!


Karl B. Andersen
Journeyman Smith
0

#2 User is offline   Ed Street 

  • Advanced Forum Member
  • PipPipPipPip
  • Group: Members
  • Posts: 52
  • Joined: 31-May 12
  • LocationPhenix City, AL
  • ABS Rating:Apprentice Smith

Posted 04 June 2012 - 08:16 PM

Great video, thanks for posting that, was very educational and helpful.