There are many types of wood that are used for knife handles. Wood that has not been stabilized often requires a stain to display the grain, plus a top coat finish to protect it. Many of the exotic woods have a lot of oil in them, so do not accept oil based finishes well.
What do you use to dye/stain different types of wood handles? What finish materials do you use for different types of woods?
Tips on sanding the handle material and filling the wood grain. What sandpaper and/or polishing materials and techniques do you use for the final finish? What methods do you use for filing the pores in the wood grain for different types of wood?
Page 1 of 1
Wood Handle Finishing - Topic For June 2012 Wood handle - dyeing, sanding and finishes
#1
Posted 01 June 2012 - 06:15 AM
Steve Culver
ABS Master Bladesmith
President: Kansas Custom Knifemaker's Association
Blade Show Table 11-S
steve@culverart.com
www.culverart.com
www.kansasknives.org
ABS Master Bladesmith
President: Kansas Custom Knifemaker's Association
Blade Show Table 11-S
steve@culverart.com
www.culverart.com
www.kansasknives.org
#2
Posted 01 June 2012 - 06:56 AM
Steve, this is another great Topic of the Month. I like and have used highly figured curly maple in knife handles. I want to pass on a few tips that I learned about curly maple over the years.
I asked Bill Moran several years ago at the Blade Show in Atlanta what he used to color his curly maple handles and he told me that he used medium or dark brown Fiebing's leather dye to color his handles. He also told me that sometimes he would mix in just a drop of red Fiebings dye in the application bottle.
I have also learned that Bill Moran had purchased the curly maple for his knives from Wayne Dunlap in Chantilly, Virginia. I first went to Wayne Dunlap's shop with Master Smith Jack Fuller who had last gone there with Bill Moran several years before. The curly maple and several other hardwoods that he has on hand are highly figured and some of the best available anywhere. Wayne has a special for knife makers which is his $100 box of highly figured handle material. http://www.dunlapwoodcrafts.com/
If you are using curly maple for your handle material then Majestic Maple Stain which is chromic acid and tap water is very helpful to really bring out the figure in the wood. You can obtain it from R.W. Wilson, P.O. Box 2012, Weirton, West Virginia 26062 or telephone 304-723-2771.
Also, Keith Casteel is nationally known for his fine engraving work on firearms and the carving of rifle stocks. Keith produces and sells his own wood oil finish which is an outstanding product and costs about $5 a bottle and can be contacted at Keith Casteel, Rt. #1, Bruceton Mills, West Virginia 26525, telephone 304-379-8309, or Email hawkeyecasteel@citlink.net
If you call R.W. Wilson or Keith Casteel to order you will find that they both are a wealth of knowledge in the finishing of curly maple.
Dan Cassidy
ABS Webmaster and Forum Administrator
Send an email to Dan

ABS Webmaster and Forum Administrator
Send an email to Dan

#3
Posted 01 June 2012 - 07:48 AM
Good topic Steve. I am interested to see the methods everyone has for different types of wood.
I have used curly maple and do use Bill Moran's method with the feibings dye. You have to keep an eye on the raised grain with maple. Hopefully Mike Williams will reply with his method for maple. His handles turn out great.
I do like the exotic woods such as ironwood which is a favorite. Always keep in mind with wood is that the sanding and sawdust is not good for you, especially with some woods ( ironwood), and always wear a respirator. I usually hand sand the ironwood to 1500 grit then go to a white scotchbrite pad. After that I will use 3M polishing papers to really bring out the luster. These are available from Rio Grande and go up to like 10,000 grit. After sanding I will apply a good paste wax and buff lightly with a clean cloth or a clean buff. The customer can then just re-apply the paste wax every so often and keep the handle looking good.
I am sure I will think of more. Headed out to the shop.
Brion
I have used curly maple and do use Bill Moran's method with the feibings dye. You have to keep an eye on the raised grain with maple. Hopefully Mike Williams will reply with his method for maple. His handles turn out great.
I do like the exotic woods such as ironwood which is a favorite. Always keep in mind with wood is that the sanding and sawdust is not good for you, especially with some woods ( ironwood), and always wear a respirator. I usually hand sand the ironwood to 1500 grit then go to a white scotchbrite pad. After that I will use 3M polishing papers to really bring out the luster. These are available from Rio Grande and go up to like 10,000 grit. After sanding I will apply a good paste wax and buff lightly with a clean cloth or a clean buff. The customer can then just re-apply the paste wax every so often and keep the handle looking good.
I am sure I will think of more. Headed out to the shop.
Brion
Brion Tomberlin
Anvil Top Custom Knives
ABS Mastersmith
Anvil Top Custom Knives
ABS Mastersmith
#4
Posted 02 June 2012 - 06:33 AM
I'm looking forward to reading this topic. I'm sure there will be a lot of good information. As for dealing with raised grain on maple, or any other wood, use some 0000 steel wool to rub against the raised grain. Going against the grain will shear off the little whiskers. If you go with the grain you will just push it down and it will eventually raise again. I like to slightly dampen the wood with a wet paper towel and then hold it over a stove eye or other heat source to raise the grain. Just warm it, don't let it burn. Then use the steel woold to remove it. Some times you have to do this several times, but the wood will come out as slick as glass.
Dale
Dale
Dale Huckabee
Journeyman Smith
dalehuckabeeknives.weebly.com
Journeyman Smith
dalehuckabeeknives.weebly.com
#5
Posted 02 June 2012 - 10:10 AM
I'm ABS apprentice level - and have only made a dozen or so knives. I like making kitchen knives because I can use them on a regular basis. I love wood handles, so a finish for wood that survives in the kitchen (excluding the dishwasher) is a personal quest.
Last year I did a "wood in the kitchen" test involving many iterations of soaks in hot soapy water, rinse, dry, repeat: http://knifedogs.com...-Kitchen-a-test
The winners of that test were:
Permalyn
Tru-Oil
a combo of Spar Urethane/Linseed Oil/Turpentine
and Safflower Oil
I'm fond of the Spar/Lin/Turp combo.
I am setting up to do a follow-on test with several finishes that I did not have in the first round and am interested in suggestions. I realize this is only one small side of wood handle finishing - but it is of interest to me, and maybe others. I'm betting ABS folks have some favorite formulas!
Last year I did a "wood in the kitchen" test involving many iterations of soaks in hot soapy water, rinse, dry, repeat: http://knifedogs.com...-Kitchen-a-test
The winners of that test were:
Permalyn
Tru-Oil
a combo of Spar Urethane/Linseed Oil/Turpentine
and Safflower Oil
I'm fond of the Spar/Lin/Turp combo.
I am setting up to do a follow-on test with several finishes that I did not have in the first round and am interested in suggestions. I realize this is only one small side of wood handle finishing - but it is of interest to me, and maybe others. I'm betting ABS folks have some favorite formulas!
#6
Posted 02 June 2012 - 04:52 PM
I am on forged knife number 9. I like Hondurian Rosewood, Purpleheart, and Black Ash mainly. I have collected about 100 or so sets of handle materials to date.
I finish my not stablized wood with Tung Oil. I form them to profile with my band saw, shape them with 220 grit, sand to 600 grit. Then I start with a fined scot-bright belt, move on to a plain cork belt. After the cork I rub them down with a a damp paper towel. Heat lightly with my torch, followed with 0000 steel wool against the grain. I do this 3 times. Now comes the Tung Oil 3 to 6 coats steel wool between each coat. Followed by 2 coats of Howards Feed-N-Wax Wood Polish and Conditioner, and another plain cork belt low speed polish.
I advise my first 2 clients to wipe and rub polish there handle every 6 months with Howards Feed-N-Wax Wood Polish and Conditioner to presever the wood.
I also stablize some of my wood using a brake vacumum system as described in the Handle and Guards Book, picture of my mason jar chamber with two pieces of maple in it which I dovetailed on to a piece of blackwood I got from Pop's for a handle on an 8" knife. (first forged knife sold, after that I started taking photos of my work)
[attachment=690:VacumumChamber.jpg]
I finish my not stablized wood with Tung Oil. I form them to profile with my band saw, shape them with 220 grit, sand to 600 grit. Then I start with a fined scot-bright belt, move on to a plain cork belt. After the cork I rub them down with a a damp paper towel. Heat lightly with my torch, followed with 0000 steel wool against the grain. I do this 3 times. Now comes the Tung Oil 3 to 6 coats steel wool between each coat. Followed by 2 coats of Howards Feed-N-Wax Wood Polish and Conditioner, and another plain cork belt low speed polish.
I advise my first 2 clients to wipe and rub polish there handle every 6 months with Howards Feed-N-Wax Wood Polish and Conditioner to presever the wood.
I also stablize some of my wood using a brake vacumum system as described in the Handle and Guards Book, picture of my mason jar chamber with two pieces of maple in it which I dovetailed on to a piece of blackwood I got from Pop's for a handle on an 8" knife. (first forged knife sold, after that I started taking photos of my work)
[attachment=690:VacumumChamber.jpg]
"Whoever pursues righteousness and love finds life, prosperity and honor"

George B. Brackett, Jr.
Apprentice Smith
Tactically Sharp, Inc.
Hialeah, FL
Tactically Sharp, Inc.

George B. Brackett, Jr.
Apprentice Smith
Tactically Sharp, Inc.
Hialeah, FL
Tactically Sharp, Inc.
#7
Posted 25 June 2012 - 12:56 PM
I like the Lockwood dyes and the Lockwood website has some nice "how to" webpages. These are either water or alcohol based dyes. I have used both in the past. Often it is the same dry dye mixed with either. The alcohol dyes seem to penetrate (depth) some hardwoods better than water based dyes. The water based dyes stay wet longer and can raise the grain on some woods such as maple. This requires re-sanding and may re-application of dye. It is just different and you can always wet the wood first, then sand, then dye.
My trouble is finding a color I like that works on different woods. Keep a notebook on your process. Keep track of the mix, the dye colors, the wood, the final sanding grit, etc. I have found that you can always go darker but not lighter unless you want to sand it all down again.
Dan
My trouble is finding a color I like that works on different woods. Keep a notebook on your process. Keep track of the mix, the dye colors, the wood, the final sanding grit, etc. I have found that you can always go darker but not lighter unless you want to sand it all down again.
Dan
Dan Petersen
Master Smith
Master Smith
#8
Posted 25 June 2012 - 01:38 PM
i think that many of the problems that we as knifemakers face; is our detirmination to continually reinvent the wheel. It is in our phyche that only I can truley do the wheel justice.
For wood finishing I think the best guys out there are the gun guys. These guys have been finishing wood to withstand heat,cold, sweat, and grizzeled bar attacks for the last several hundred years. AND, make it look good to boot.
Get a book on finishing gunstocks. Use their techniques. Then improve on it if you can. If you ever get a chance to go to the custom gunmakers guild show; you can see that they do know how to finish wood.
90% of the crappy wood finishes I saw at Atlanta was not the stain; but the filling and finish that was on top of the stain.
Just a thought from the oven called Oklahoma.
M
For wood finishing I think the best guys out there are the gun guys. These guys have been finishing wood to withstand heat,cold, sweat, and grizzeled bar attacks for the last several hundred years. AND, make it look good to boot.
Get a book on finishing gunstocks. Use their techniques. Then improve on it if you can. If you ever get a chance to go to the custom gunmakers guild show; you can see that they do know how to finish wood.
90% of the crappy wood finishes I saw at Atlanta was not the stain; but the filling and finish that was on top of the stain.
Just a thought from the oven called Oklahoma.
M
Mike Williams
Master Smith
Master Smith
#9
Posted 01 July 2012 - 05:01 AM
For the non-exotic/oily woods, I have used a gunstock finish from Brownell's for several years with very good results. It is called Pro Oil and is a combination of boiled linseed oil & urethane. I find that the urethane adds a harder finish but it applies much the same as a simple oil finish. I will apply a coat of it and when partially dry, 10-15 minutes, buff with a clean soft cloth then allow to fully cure before applying the next coat. This will eventually fill the pores through multiple coats and leave a glossy finish. If you want a less glossy finish then apply a coat of wax (after the last coat of finish has cured). I usually will apply 6-8 coats over a two/three day period.
Gary
Gary
Gary Mulkey