Hey everyone!

Here is a series of five videos showing how I made and tested my MS performance test knife. I hope you all like them, enjoy!




Kyle Royer, Master Smith
0

#2 User is online   Kyle Royer 

  • Forum Member
  • PipPip
  • Group: Members
  • Posts: 17
  • Joined: 07-June 11
  • LocationMountain View, MO
  • ABS Rating:Master Smith

Posted 18 March 2012 - 06:07 PM




Kyle Royer, Master Smith
0

#3 User is online   Kyle Royer 

  • Forum Member
  • PipPip
  • Group: Members
  • Posts: 17
  • Joined: 07-June 11
  • LocationMountain View, MO
  • ABS Rating:Master Smith

Posted 18 March 2012 - 06:08 PM



Thanks for watching! Now get out there and take your JS or MS performance test! :D
Kyle Royer, Master Smith
0

#4 User is online   ABS Webmaster 

  • Administrator
  • Icon
  • View gallery
  • Group: Administrators
  • Posts: 909
  • Joined: 21-December 09
  • LocationSalida, Colorado
  • ABS Rating:Journeyman Smith

Posted 18 March 2012 - 06:54 PM

Kyle:

Thank you for posting your videos. They are very well done and will be helpful to many.

Dan Cassidy
ABS Webmaster and Forum Administrator

Send an email to Dan

Posted Image


0

#5 User is offline   Jonathan Stanley 

  • Advanced Forum Member
  • PipPipPipPip
  • View gallery
  • Group: Members
  • Posts: 156
  • Joined: 07-March 12
  • LocationHot Springs Arkansas
  • ABS Rating:Apprentice Smith

Posted 19 March 2012 - 03:42 PM

Wow, :lol:
Thanks so much for posting that. :)
I really learned a lot. :)
Jonathan Stanley
Apprentice Smith
0

#6 User is offline   Jason_E_Stone 

  • Active Forum Member
  • PipPipPip
  • Group: Members
  • Posts: 24
  • Joined: 04-February 12
  • LocationAndrews, South Carolina
  • ABS Rating:Apprentice Smith

Posted 20 March 2012 - 10:49 PM

Congratulation and thanks for the videos, they are informative. :)
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users