Forrest Bowie Questions on dimensions of the original

#1 User is offline   Geoff Keyes 

  • Forum Member
  • PipPip
  • Group: Members
  • Posts: 5
  • Joined: 11-June 10
  • LocationDuvall, WA
  • ABS Rating:Journeyman Smith

Posted 29 July 2011 - 04:26 PM

Hi folks,

I recently finished a version of the Forrest bowie. I got the overall effect I was after, but I'm thinking that I missed the thickness of the original. I've been unable to track down a detailed description of the knife. Does anyone have any information that I can use to get closer? Does anyone know the location of the original, or leads I might follow to track down more info?

Here is my version

Attached File  Keyes1WEB.jpg (47.71K)
Number of downloads: 11

BL 10 1/4"
OL 15 3/4"
Blade 1084 (forged from a 3" round)
Handle Walnut

and here is the original

Attached File  Keyes2WEB.jpg (17.16K)
Number of downloads: 1

Mine is shorter by about 3 inches, and is very light and thin (about 0.130 at the handle). This is also my first attempt at checkering.

Thanks for your help with this,

Geoff Keyes JS
Geoff Keyes
5 Elements Forge
Duvall, WA

ABS Journeyman
0

#2 User is offline   Ricky Bunn 

  • New Forum Member
  • Pip
  • Group: Members
  • Posts: 3
  • Joined: 30-October 10
  • ABS Rating:Apprentice Smith

Posted 03 April 2012 - 05:11 PM

the forrest bowie has a maximun thickness of 5/16 and a severly tapered tang. the blade is 12 3/16 long by 1.75 inches wide. the deep cut checkering is app. 8 lines per inch and the angle between the lines is 90 degrees. the scales are attached with 3 silver birds-eye rivets and washers. the pommel cap is missing and I think the handle is now about 5 inches. a great artical in March 2010 Blade by Jim Batson
0

#3 User is offline   Lin Rhea 

  • Advanced Forum Member
  • PipPipPipPip
  • View gallery
  • Group: Members
  • Posts: 436
  • Joined: 04-February 10
  • LocationPrattsville, Arkansas
  • ABS Rating:Master Smith

Posted 03 April 2012 - 05:15 PM

Hey Ricky! Sure glad to see you hangin around here!
Lin Rhea, ABS Mastersmith
Email me
0

#4 User is offline   Mike Williams 

  • Advanced Forum Member
  • PipPipPipPip
  • View gallery
  • Group: Members
  • Posts: 105
  • Joined: 23-February 10
  • LocationBroken Bow, Oklahoma
  • ABS Rating:Master Smith

Posted 04 April 2012 - 03:58 AM

Hey Ricky!!!

Good to see the more intellectual side of the knife world posting here.

take care
M
Mike Williams
Master Smith