Posted 22 May 2011 - 02:10 PM

Well, it's been a long time coming... As it worked out, I had to loose my job, be "unemployed" for a year and a half, find a new job being paid half of what I had been, be asked to relocate to Boise, call my long time friend Bill Burke to see how he's doing, get invited to a weekend "Open shop" at his place, buy a 2X4, beg what turned out to be 10 inches of rope and some lanyard string and bring my test knife that I made over a year ago in order to get around to doing the JS performance test. Man, if the nerves I had at Bill's are any indication of what it will be like (times 50, I'm sure) when I submit knives for judging, I'm going to have to have a pacemaker installed just to survive...

Well, to make a long story longer, two attempts at the rope, what seemed like half an hour of chopping, a bald spot on my arm and some tense moments with a cheater-pipe on the handle of my knife, I can finally say... Whew! It's over, my test knife passed the performance test. Now It's time to start making 5 or 6 more knives for the judging portion of the test.

Enough of that though, because I really want this thread to be about those that have helped me along my way. If it were't for the internet and all of you here, Bill Burke and all of his selfless support and coaching over the years, I don't know if I'd have been able to have passed the performance test. My hat is off to you All... Thanks Everyone! It was nerve wracking, but a heck of a lot of fun yesterday! I wish I had some pictures to post... Maybe, when the camera gets unpacked I can post a picture of my crooked knife... About all it's good for now is cutting corners! Posted Image

Thanks again Bill for having me over yesterday! The Quigley shoot was a great topper to a fantastic day!
0

#2 User is offline   Lin Rhea 

  • Advanced Forum Member
  • PipPipPipPip
  • View gallery
  • Group: Members
  • Posts: 437
  • Joined: 04-February 10
  • LocationPrattsville, Arkansas
  • ABS Rating:Master Smith

Posted 22 May 2011 - 05:50 PM

Congratulations Rick!
Lin Rhea, ABS Mastersmith
Email me
0

#3 User is offline   Dale Huckabee 

  • Advanced Forum Member
  • PipPipPipPip
  • View gallery
  • Group: Members
  • Posts: 121
  • Joined: 31-May 10
  • LocationMaylene, Alabama
  • ABS Rating:Journeyman Smith

Posted 22 May 2011 - 07:56 PM

Congradulations Rick.

For me the test was more nerve racking than the judging at Atlanta. By then I was just ready for it to be over, regardless of the outcome.

Dale
Dale Huckabee
Journeyman Smith
dalehuckabeeknives.weebly.com
0

#4 User is offline   BrionTomberlin 

  • Administrator
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 591
  • Joined: 28-December 09
  • LocationNorman, Oklahoma
  • ABS Rating:Master Smith

Posted 22 May 2011 - 08:25 PM

Congratulations Rick, well done! Just think you will have lots of company when you present your knives and they will be feeling the same way. Nerve wracking, yes, but what a feeling when you pass and float through the rest of the weekend. Congrats again.
Brion
Brion Tomberlin
Anvil Top Custom Knives
ABS Mastersmith
0

#5 User is offline   ABS Webmaster 

  • Administrator
  • Icon
  • View gallery
  • Group: Administrators
  • Posts: 909
  • Joined: 21-December 09
  • LocationSalida, Colorado
  • ABS Rating:Journeyman Smith

Posted 22 May 2011 - 09:46 PM

Congratulations Rick!

I agree with Dale.
Dan Cassidy
ABS Webmaster and Forum Administrator

Send an email to Dan

Posted Image


0

#6 User is offline   Steve Culver 

  • Administrator
  • Icon
  • View gallery
  • Group: Administrators
  • Posts: 378
  • Joined: 29-December 09
  • LocationMeriden, KS
  • ABS Rating:Master Smith

Posted 23 May 2011 - 07:32 AM

Congratulations Rick!!! We'll see you in Atlanta!
Steve Culver
ABS Master Bladesmith
President: Kansas Custom Knifemaker's Association
Blade Show Table 11-S
steve@culverart.com
www.culverart.com

www.kansasknives.org
0

#7 User is offline   Rick Baum 

  • Advanced Forum Member
  • PipPipPipPip
  • Group: Members
  • Posts: 168
  • Joined: 11-March 10
  • LocationIdaho (Boise)
  • ABS Rating:Apprentice Smith

Posted 23 May 2011 - 05:23 PM

Thanks for the kind words and encouragement! I really appreciate it. I sure hope Dale and Dan are right because my old ticker needs a rest after yesterday. :)

Thanks guys!
0

#8 User is offline   Bob Hartman 

  • Forum Member
  • PipPip
  • Group: Members
  • Posts: 13
  • Joined: 09-May 10
  • LocationBoise, id
  • ABS Rating:Apprentice Smith

Posted 24 May 2011 - 02:55 PM

I happened to be at Bill's when Rick tested. He, and his knife performed flawlessly. Congratulations again Rick. It was great meeting you.
0

#9 User is offline   Dan Hockensmith 

  • Active Forum Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 40
  • Joined: 01-February 11
  • LocationBerthoud, Colorado
  • ABS Rating:Journeyman Smith

Posted 25 May 2011 - 09:22 PM

Good job Rick! Congratulations! Dan
0

#10 User is offline   Rick Baum 

  • Advanced Forum Member
  • PipPipPipPip
  • Group: Members
  • Posts: 168
  • Joined: 11-March 10
  • LocationIdaho (Boise)
  • ABS Rating:Apprentice Smith

Posted 31 May 2011 - 02:28 PM

Thanks Dan and Bob!

Bob, Likewise, it was great meeting you too. I hope we can get together again soon.
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users