Planning And Designing The 2010 Journeyman Smith Knife Of The Year Part 2 of 2

#1 User is online   ABS Webmaster 

  • Administrator
  • Icon
  • View gallery
  • Group: Administrators
  • Posts: 904
  • Joined: 21-December 09
  • LocationSalida, Colorado
  • ABS Rating:Journeyman Smith

Posted 07 April 2011 - 03:26 PM

"Planning and Designing the 2010 Journeyman Smith Knife of the Year"
Part 2 of 2
by Brian Thie, Journeyman Smith



Brian Thie made the 2010 Journeyman Smith Knife of the Year. It was auctioned at the 2010 Atlanta Blade Show at the ABS Knife Auction to help raise funds for the American Bladesmith Society. Thank you Brian!

This is the second and most important article in this series. It features many techniques and is very well written. The article is in a PDF or Adobe Acrobat file format because it has many photos, is eleven (11) pages long, and can be more easily downloaded and printed in this format.

The article can be accessed at, CLICK:
Attached File  Thie-Planning and Designing the 2010 JS Knife of the Year-Part2-1.pdf (817.64K)
Number of downloads: 78

Attached File  2010-JS-Knife-Brian-Thie.jpg (44.37K)
Number of downloads: 3



Dan Cassidy
ABS Webmaster and Forum Administrator

Send an email to Dan

Posted Image


0

#2 User is offline   Jim Poling 

  • New Forum Member
  • Pip
  • Group: Members
  • Posts: 3
  • Joined: 08-August 10
  • LocationAlvarado MN
  • ABS Rating:Journeyman Smith

Posted 19 June 2011 - 07:14 AM

Hi Brian

Outstanding articles! Thanks for taking the time to share your processes and journey to complete this beautiful knife. It is always fun and encouraging to see how others get it done. I definitely picked up some tricks from your article.

Thanks
Jim