Several Candidates Pass Performance Test In Washington State Under Supervision of Master Smiths Rader and Ferry

#1 User is offline   Dan Cassidy 

  • Administrator
  • Icon
  • View gallery
  • Group: Administrators
  • Posts: 2,069
  • Joined: 21-December 09
  • LocationColorado Rockies
  • ABS Rating:Journeyman Smith

Posted 10 March 2011 - 08:50 PM

Several Candidates Pass Performance Test in Washington State


We have news that several candidates for Journeyman Smith: ABS Apprentices Daniel Erickson and Rick Lucas, and JS Geoff Keyes who is a candidate for Master Smith have passed their Performance Tests. The tests were administered by Master Smiths Michael Rader and Tom Ferry in Washington State.

Below is a video clip on YouTube of the event and the performance test of Daniel Erickson.

Congratulations gentlemen!



Dan Cassidy
ABS Forum Administrator
Journeyman Smith

Send an email to Dan

Posted Image


0

#2 User is offline   Phil Dwyer 

  • Advanced Forum Member
  • PipPipPipPip
  • Group: Members
  • Posts: 296
  • Joined: 04-February 10
  • LocationHonolulu
  • ABS Rating:Apprentice Smith

Posted 10 March 2011 - 11:46 PM

Congratulations gentleman!!! Where in WA?
Phil Dwyer
Earth Crafts & Applied Arts
www.eartharts.us (update pending)
0

#3 User is offline   Barry Clodfelter 

  • Active Forum Member
  • PipPipPip
  • Group: Members
  • Posts: 42
  • Joined: 07-March 11
  • LocationDavidson, NC
  • ABS Rating:Apprentice Smith

Posted 11 March 2011 - 05:19 AM

Congratulations guys!!
0

#4 User is offline   BrionTomberlin 

  • Administrator
  • Icon
  • View gallery
  • Group: Administrators
  • Posts: 1,359
  • Joined: 28-December 09
  • LocationNorman, Oklahoma
  • ABS Rating:Master Smith

Posted 11 March 2011 - 07:21 AM

Congratulations guys. Well done. I look forward to seeing you all in Atlanta.
Brion
Brion Tomberlin
Anvil Top Custom Knives
ABS Mastersmith
0

#5 User is offline   Lin Rhea 

  • Advanced Forum Member
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,180
  • Joined: 04-February 10
  • LocationPrattsville, Arkansas
  • ABS Rating:Master Smith

Posted 11 March 2011 - 07:25 AM

This is great for all to see. Congratulations. Lin
Lin Rhea, ABS Mastersmith
Email me
www.rheaknives.com
0

#6 User is offline   Allen Newberry 

  • Advanced Forum Member
  • PipPipPipPip
  • View gallery
  • Group: Members
  • Posts: 194
  • Joined: 18-May 10
  • LocationN.W. Arkansas
  • ABS Rating:Apprentice Smith

Posted 11 March 2011 - 08:22 AM

Way to go guys! I'll be keeping an eye out to see what you guys come up with for Atlanta/San Antonio.
0

#7 User is offline   Rick Baum 

  • Advanced Forum Member
  • PipPipPipPip
  • Group: Members
  • Posts: 168
  • Joined: 11-March 10
  • LocationIdaho (Boise)
  • ABS Rating:Apprentice Smith

Posted 11 March 2011 - 12:53 PM

Congrat's All!
0

#8 User is offline   Daniel Erickson 

  • New Forum Member
  • Pip
  • Group: Members
  • Posts: 4
  • Joined: 11-March 11
  • LocationSnomish Wa
  • ABS Rating:Journeyman Smith

Posted 11 March 2011 - 11:06 PM

View PostPhil Dwyer, on 10 March 2011 - 11:46 PM, said:

Congratulations gentleman!!! Where in WA?

Rick and I are from Snohomish Wa. Geoff (tested for MS) is from Duvall Wa. About 30-45 min NE of Seattle.
Daniel Erickson
Ring of Fire Forge
0

#9 User is offline   Daniel Erickson 

  • New Forum Member
  • Pip
  • Group: Members
  • Posts: 4
  • Joined: 11-March 11
  • LocationSnomish Wa
  • ABS Rating:Journeyman Smith

Posted 11 March 2011 - 11:15 PM

Thank you for your encouraging comments. I will be getting my presentation knives ready and hope to attend the San Antonio show in January.
Daniel Erickson
Ring of Fire Forge
0

#10 User is offline   Bruce Bingenheimer 

  • Active Forum Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 22
  • Joined: 09-March 10
  • LocationSpring Creek, Nevada
  • ABS Rating:Journeyman Smith

Posted 12 March 2011 - 06:55 PM

Congrats all to all of you. I got real excited watching that you-tube Daniel. Now you all get to enjoy the rest of the journey. Looking foward to those testing in San Antonio.