Burt Foster Wins Battle Of The Bladesmiths 4th Great Smoky Mountain Bladesmithing Symposium

#1 User is offline   Dan Cassidy 

  • Administrator
  • Icon
  • View gallery
  • Group: Administrators
  • Posts: 1,942
  • Joined: 21-December 09
  • LocationColorado Rockies
  • ABS Rating:Journeyman Smith

Posted 04 March 2011 - 08:00 PM

"Battle of the Bladesmiths" at the Great Smoky Mountain Symposium


The Second American Bladesmith Society "Battle of the Bladesmiths" was conducted this evening, March 4th, at the Great Smoky Mountain Bladesmithing Symposium and was won by Master Smith Burt Foster. The hard fought contest was conducted before an enthusiastic crowd at Haywood Community College in Clyde, North Carolina. The contestants included American Bladesmith Society Master Smiths Joe Keeslar, Jason Knight, Jim Rodebaugh, and Burt Foster.

The Great Smoky Mountain Bladesmithing Symposium began today and will continue through Sunday, March 6th. ABS Store Manager Cindy Sheely emailed the results of the contest and the below photos to me.

Attached Image
Burt Foster and BR Hughes

Attached Image
Bill Wiggins and Joe Keeslar

Attached Image
Jim Rodebaugh
Attached Image

The contest knives..Clockwise starting lower right: Keeslar, Foster, Knight, and Rodebaugh

Dan Cassidy
Journeyman Smith

Send an email to Dan

Posted Image


0

#2 User is offline   Lin Rhea 

  • Advanced Forum Member
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,076
  • Joined: 04-February 10
  • LocationPrattsville, Arkansas
  • ABS Rating:Master Smith

Posted 05 March 2011 - 09:39 AM

Congratulations to Burt.

I find it interesting that I think I can recognize each of these makers work within these four knives even though their names are not posted, that I can see.

Clockwise starting lower right: Keeslar, Foster, Knight, and Rodebaugh

Correct me if I'm wrong.
Lin Rhea, ABS Mastersmith
Email me
www.rheaknives.com
0

#3 User is offline   Dan Cassidy 

  • Administrator
  • Icon
  • View gallery
  • Group: Administrators
  • Posts: 1,942
  • Joined: 21-December 09
  • LocationColorado Rockies
  • ABS Rating:Journeyman Smith

Posted 05 March 2011 - 10:01 AM

Lin:

You are correct in your pairing of the Master Smiths with their contest knives and I added it to the photo caption in my post above after your observation. You have a good eye for detail.

Dan Cassidy
Journeyman Smith

Send an email to Dan

Posted Image


0

#4 User is offline   Rick Baum 

  • Advanced Forum Member
  • PipPipPipPip
  • Group: Members
  • Posts: 168
  • Joined: 11-March 10
  • LocationIdaho (Boise)
  • ABS Rating:Apprentice Smith

Posted 05 March 2011 - 05:12 PM

Congratulations to Burt!

At the risk of sounding ignorant, which I am :), what was the criteria of the contest?
0

#5 User is offline   Dan Cassidy 

  • Administrator
  • Icon
  • View gallery
  • Group: Administrators
  • Posts: 1,942
  • Joined: 21-December 09
  • LocationColorado Rockies
  • ABS Rating:Journeyman Smith

Posted 05 March 2011 - 08:41 PM

Hammer In Update

The cutting demonstration results from this evening are in. Burt Foster won first place and Jason Knight and Bill Wiggins tied for second place.

Attached Image
Jim Batson presenting first place award to Burt Foster

Attached Image

Jason Knight, Jim Batson, Bill Wiggins, Greg Neely, and Jim Rodebaugh

Dan Cassidy
Journeyman Smith

Send an email to Dan