American Bladesmith Society Forum: My Journeyman Smith Cutting And Bending Test - American Bladesmith Society Forum

Jump to content

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

My Journeyman Smith Cutting And Bending Test

#1 User is offline   Mariano Gugliotta 

  • Forum Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 19
  • Joined: 20-May 10
  • LocationBuenos Aires Argentina
  • ABS Rating:Apprentice Smith

Posted 22 September 2010 - 10:21 AM

Hi, last September 20th was very special for me. After years I finally took my JS performance test at MS Rodrigo Sfreddo shop in Nova Petropolis, Brasil.

I passed the test Posted Image

Posted Image

Posted Image

A good friend, Manuel Quiroga, took this video of the test.



This part has an edition problem, I will re make the video soon..


Mariano Gugliotta
0

#2 User is offline   Mariano Gugliotta 

  • Forum Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 19
  • Joined: 20-May 10
  • LocationBuenos Aires Argentina
  • ABS Rating:Apprentice Smith

Posted 22 September 2010 - 10:21 AM

Last part





Hope you like these videos and thank you all for the technical advices and support.

Saludos

Mariano
Mariano Gugliotta
0

#3 User is offline   BrionTomberlin 

  • Administrator
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 608
  • Joined: 28-December 09
  • LocationNorman, Oklahoma
  • ABS Rating:Master Smith

Posted 22 September 2010 - 07:38 PM

Mariano, Congratulations. Excellent videos. Very well done and a nice bend. Great job and congratulations again. I look forward to seeing you in Atlanta and meeting you in person.
Best regards
Brion
Brion Tomberlin
Anvil Top Custom Knives
ABS Mastersmith
0

#4 User is offline   ABS Webmaster 

  • Administrator
  • Icon
  • View gallery
  • Group: Administrators
  • Posts: 936
  • Joined: 21-December 09
  • LocationSalida, Colorado
  • ABS Rating:Journeyman Smith

Posted 22 September 2010 - 08:37 PM


Mariano
Congratulations! I look forward to seeing you in Atlanta when you present your knives.
Also, thank you to Mastersmith Rodrigo Sfreddo for administering the JS performance test in Brazil.
Dan Cassidy
ABS Webmaster and Forum Administrator

Send an email to Dan

Posted Image


0

#5 User is offline   Phil Dwyer 

  • Advanced Forum Member
  • PipPipPipPip
  • Group: Members
  • Posts: 206
  • Joined: 04-February 10
  • LocationHonolulu
  • ABS Rating:Apprentice Smith

Posted 22 September 2010 - 10:06 PM

That's GREAT Mariano!

Well done. How many times did you have cut the wood in half? It must have have been nice to have all your friends there. It was fun watching them all celebrating the moment with you at the end. Thanks for sharing it with us too!

All the best, Phil
Phil Dwyer
Earth Crafts & Applied Arts
www.eartharts.us (update pending)
0

#6 User is offline   Mariano Gugliotta 

  • Forum Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 19
  • Joined: 20-May 10
  • LocationBuenos Aires Argentina
  • ABS Rating:Apprentice Smith

Posted 23 September 2010 - 05:33 AM

Thanks!

I´m working on my 5 presentation knives for Atlanta 2011.

MS Sfreddo is a magnificent bladesmith and a great person.

The people in the video were friends of mine and Rodrigo Sfreddo´s students.

It was all very exciting and emotional.

The blade was able to cut wood 4 times, rope 6 times , and shaved my arm 2 times, then bent 90 ° without breaking the edge.

Saludos and thanks to all!

Mariano
Mariano Gugliotta
0

#7 User is online   Lin Rhea 

  • Advanced Forum Member
  • PipPipPipPip
  • View gallery
  • Group: Members
  • Posts: 451
  • Joined: 04-February 10
  • LocationPrattsville, Arkansas
  • ABS Rating:Master Smith

Posted 25 September 2010 - 07:12 PM

Watching that brought it all back. The tension, the worry, the excitement, but also the celebration. Well done. By the way, I was present at Rodrigo's JS test and it was the same excitement then too. Congratulations. Lin
Lin Rhea, ABS Mastersmith
Email me
0

#8 User is offline   Rick Baum 

  • Advanced Forum Member
  • PipPipPipPip
  • Group: Members
  • Posts: 168
  • Joined: 11-March 10
  • LocationIdaho (Boise)
  • ABS Rating:Apprentice Smith

Posted 29 September 2010 - 04:26 PM

Congrat's Mariano! Nice job... Looks like everyone had a good time... I imagine it feels pretty good to have that portion of the test out of the way. Not that you will need it based on the work that I have seen from you, but, good luck in Atlanta! Hopefully I will see you there next spring.

RIck
0

#9 User is offline   Allen Newberry 

  • Advanced Forum Member
  • PipPipPipPip
  • View gallery
  • Group: Members
  • Posts: 157
  • Joined: 18-May 10
  • LocationN.W. Arkansas
  • ABS Rating:Apprentice Smith

Posted 29 September 2010 - 05:21 PM

Way to go! And thanks for posting up the videos so we could all share in your excitement.