52100 Drop Point Hunter by Ed Caffrey, MS, "The Montana Bladesmith"
Image Information
- Views: 837
- Comments: 0
- File Size: 28.19K
- Dimensions: 400x306
- Camera Data: View EXIF properties
Copyright
© "The Montana Bladesmith"
4" blade of differentially heat treated 52100, Nickel Silver guard and multiple spacers, engraved guard, and Sambar Stag handle