by Jerry Bennett and Dan Petersen
This is an unusual knife in that the steel was melted using a thermite charged furnace and is a niobium alloy. The steel was made by Jerry Bennett and a knife was made from the steel by Dan Petersen. See the Thermite gallery for images of the process.